Salt spray testing and post-treatment comparisons for plated PPS
We compared corrosion after salt spray exposure and appearance under different post-treatments for copper- and nickel-plated PPS.
Plating development, process trials and technical reviews by SUNGJINLOGIS.
73 articles
We compared corrosion after salt spray exposure and appearance under different post-treatments for copper- and nickel-plated PPS.
We compared post-treatment, rinsing, and water removal conditions to reduce staining on finished plated parts.
We adjusted the make-up procedure for a sulfate-based trivalent chromium bath, repeated trials and checked the plated appearance.
We linked tank deposition observations with cleaning and bath replacement history to track recurrence.
We compared incomplete coverage and adhesion early and late in production, including observations before and after pretreatment changes.
We measured actual pump delivery, adjusted chemical replenishment, and tracked changes in bath concentration and coating thickness.
Plant 3 operates a developed HPPA/PPA plating process that links pretreatment with copper and nickel deposition.
We varied rack mounting and workflow for PPS panels and compared appearance, thickness on both sides, and adhesion.
We compared pH readings for fresh and post-production cleaning water alongside water replacement history.
Selective plating and blackening processes were reviewed for PC–stainless steel composite parts, and comparative tests were designed to examine reflection reduction.