Overview
We examined differences in localized unplated areas with and without a conditioner on PC specimens transferred between plants.
We examined coverage when PC pretreatment and plating were carried out across multiple plants. After transfer, drying, and repeat pretreatment, specimens were plated with or without a conditioner.
Specimen photographs and appearance were compared after electroless nickel plating. Specimens treated with the conditioner showed fewer localized unplated areas near the edges.