Overview
Thickness measurements on both sides of plated PPS were reanalyzed by lot, distinguishing average thickness, local deviations and adhesion observations.
Existing PPS plating tests were reviewed by lot to examine thickness differences between the two sides. Front and back surfaces and copper and nickel layers were assessed separately by comparing averages, the difference between maximum and minimum values, and measurements outside specification.
Even in a lot with a smaller difference in average copper thickness between the front and back, localized low thickness was found in parts of the back surface. In another lot, localized excessive nickel thickness was observed on the front of parts near the end of the rack.
Appearance and cross-cut results were matched to each lot, with thickness assessments and adhesion observations documented separately. Lots with different mounting methods and process histories were distinguished when examining surface-specific distributions and local variation.